BOPP >> General printing

GRADE JP201 JP301 JP401
Properties ITEM METHOD UNIT RESULT
THICKNESS POINT 20 30 40
TENSILE
STRENGTH
MO ASTM
D-882
Mpa ≥110 ≥120
TD ≥200 ≥220
ELONGATION
AT BREAK
MO % ≤ 220 ≤ 210
TD ≤ 80 ≤ 70
HEAT
SHRINKAGE
(120℃/15min)
MO ASTM
D-1204
% ≤ 5.0 ≤ 4.5  
TD ≤ 2.0 ≤ 1.5
WET
TENSION
IN ASTM
D-2578
mN/m ≥36 ≥36
OUT      
HAZE ASTM
D-1003
% ≤1.8 ≤2.2
C.O.F IN/IN ASTM
D-1894
  ≤0.8 ≤0.7
OUT/OUT   ≤0.8 ≤0.7