| GRADE | JP201 | JP301 | JP401 | ||||
|---|---|---|---|---|---|---|---|
| Properties | ITEM | METHOD | UNIT | RESULT | |||
| THICKNESS | POINT | ㎛ | 20 | 30 | 40 | ||
| TENSILE STRENGTH | MO | ASTM D-882 | Mpa | ≥110 | ≥120 | ||
| TD | ≥200 | ≥220 | |||||
| ELONGATION AT BREAK | MO | % | ≤ 220 | ≤ 210 | |||
| TD | ≤ 80 | ≤ 70 | |||||
| HEAT SHRINKAGE (120℃/15min) | MO | ASTM D-1204 | % | ≤ 5.0 | ≤ 4.5 | ||
| TD | ≤ 2.0 | ≤ 1.5 | |||||
| WET TENSION | IN | ASTM D-2578 | mN/m | ≥36 | ≥36 | ||
| OUT | |||||||
| HAZE | ASTM D-1003 | % | ≤1.8 | ≤2.2 | |||
| C.O.F | IN/IN | ASTM D-1894 | ≤0.8 | ≤0.7 | |||
| OUT/OUT | ≤0.8 | ≤0.7 | |||||