GRADE | JM181 | JM201 | ||||
---|---|---|---|---|---|---|
Properties | ITEM | METHOD | UNIT | RESULT | ||
THICKNESS | point | ㎛ | 18 | 20 | ||
TENSILE STRENGTH |
MO | ASTM D-882 |
Mpa | ≥110 | ||
TD | ≥200 | |||||
ELONGATION AT BREAK |
MO | % | ≤ 220 | |||
TD | ≤ 80 | |||||
HEAT SHRINKAGE (120℃/15min) |
MO | ASTM D-1204 |
% | ≤ 5.0 | ||
TD | ≤ 2.0 | |||||
WET TENSION |
IN | ASTM D-2578 |
mN/m | ≥36 | ≥36 | |
OUT | ≥36 | (≥36) | ||||
HAZE | ASTM D-1003 |
% | 75±10 | |||
C.O.F | IN/IN | ASTM D-1894 |
≤0.7 | |||
OUT/OUT | ≤0.7 |