| GRADE | JM181 | JM201 | ||||
|---|---|---|---|---|---|---|
| Properties | ITEM | METHOD | UNIT | RESULT | ||
| THICKNESS | POINT | ㎛ | 18 | 20 | ||
| TENSILE STRENGTH | MO | ASTM D-882 | Mpa | ≥110 | ||
| TD | ≥200 | |||||
| ELONGATION AT BREAK | MO | % | ≤ 220 | |||
| TD | ≤ 80 | |||||
| HEAT SHRINKAGE (120℃/15min) | MO | ASTM D-1204 | % | ≤ 5.0 | ||
| TD | ≤ 2.0 | |||||
| WET TENSION | IN | ASTM D-2578 | mN/m | ≥36 | ≥36 | |
| OUT | ≥36 | (≥36) | ||||
| HAZE | ASTM D-1003 | % | 75±10 | |||
| C.O.F | IN/IN | ASTM D-1894 | ≤0.7 | |||
| OUT/OUT | ≤0.7 | |||||