GRADE | JT301 | JT401 | JT501 | ||||
---|---|---|---|---|---|---|---|
Properties | ITEM | METHOD | UNIT | RESULT | |||
THICKNESS | point | ㎛ | 30 | 40 | 50 | ||
TENSILE STRENGTH |
MO | ASTM D-882 |
Mpa | ≥120 | |||
TD | ≥220 | ||||||
ELONGATION AT BREAK |
MO | % | ≤ 210 | ||||
TD | ≤ 70 | ||||||
HEAT SHRINKAGE (120℃/15min) |
MO | ASTM D-1204 |
% | ≤ 4.5 | |||
TD | ≤ 1.5 | ||||||
WET TENSION |
IN | ASTM D-2578 |
mN/m | ≥36 | |||
OUT | |||||||
HAZE | ASTM D-1003 |
% | ≤2.2 | ≤2.5 | |||
C.O.F | IN/IN | ASTM D-1894 |
≤0.7 | ||||
OUT/OUT | ≤0.7 |