GRADE | JH201 | JH301 | ||||
---|---|---|---|---|---|---|
Properties | ITEM | METHOD | UNIT | RESULT | ||
THICKNESS | point | ㎛ | 20 | 30 | ||
TENSILE STRENGTH |
MO | ASTM D-882 |
Mpa | ≥ 110 | ||
TD | ≥ 200 | |||||
ELONGATION AT BREAK |
MO | % | ≤ 220 | |||
TD | ≤ 80 | |||||
HEAT SHRINKAGE (120℃/15min) |
MO | ASTM D-1204 |
% | ≤ 5.0 | ||
TD | ≤ 2.0 | |||||
WET TENSION |
IN | ASTM D-2578 |
mN/m | ≥ 36 | ||
OUT | ||||||
HAZE | ASTM D-1003 |
% | ≤ 2.2 | ≤ 2.5 | ||
HEAT SEALING TEMP | 2kg/1second | ℃ | 125/200g More than | 115/200g More than | ||
C.O.F | IN/IN | ASTM D-1894 |
≤ 0.5 | |||
OUT/OUT | ≤ 0.5 |