| GRADE | JH201 | JH301 | ||||
|---|---|---|---|---|---|---|
| Properties | ITEM | METHOD | UNIT | RESULT | ||
| THICKNESS | POINT | ㎛ | 20 | 30 | ||
| TENSILE STRENGTH | MO | ASTM D-882 | Mpa | ≥ 110 | ||
| TD | ≥ 200 | |||||
| ELONGATION AT BREAK | MO | % | ≤ 220 | |||
| TD | ≤ 80 | |||||
| HEAT SHRINKAGE (120℃/15min) | MO | ASTM D-1204 | % | ≤ 5.0 | ||
| TD | ≤ 2.0 | |||||
| WET TENSION | IN | ASTM D-2578 | mN/m | ≥ 36 | ||
| OUT | ||||||
| HAZE | ASTM D-1003 | % | ≤ 2.2 | ≤ 2.5 | ||
| HEAT SEALING TEMP | 2kg/1초 | ℃ | 125/200g 이상 | 115/200g 이상 | ||
| C.O.F | IN/IN | ASTM D-1894 | ≤ 0.5 | |||
| OUT/OUT | ≤ 0.5 | |||||