| GRADE | JH201 | JH301 | ||||
|---|---|---|---|---|---|---|
| Properties | ITEM | METHOD | UNIT | RESULT(대표값임) | ||
| THICKNESS(두께) | 포인트법 | ㎛ | 20 | 30 | ||
| TENSILE STRENGTH (파단인장강도)  | 
      MO | ASTM D-882  | 
      Mpa | ≥ 110 | ||
| TD | ≥ 200 | |||||
| ELONGATION AT BREAK (파단신장률)  | 
      MO | % | ≤ 220 | |||
| TD | ≤ 80 | |||||
| HEAT SHRINKAGE (120℃/15min) (가열치수변화율)  | 
      MO | ASTM D-1204  | 
      % | ≤ 5.0 | ||
| TD | ≤ 2.0 | |||||
| WET TENSION (습윤장력)  | 
      IN | ASTM D-2578  | 
      mN/m | ≥ 36 | ||
| OUT | ||||||
| HAZE (흐림도)  | 
      ASTM D-1003  | 
      % | ≤ 2.2 | ≤ 2.5 | ||
| HEAT SEALING TEMP | 2kg/1초 | ℃ | 125/200g 이상 | 115/200g 이상 | ||
| C.O.F (마찰계수)  | 
      IN/IN | ASTM D-1894  | 
      ≤ 0.5 | |||
| OUT/OUT | ≤ 0.5 | |||||