GRADE | WO | WG | ||||
---|---|---|---|---|---|---|
Properties | ITEM | METHOD | UNIT | RESULT | RESULT | |
THICKNESS | point | ㎛ | 30 | 30 | ||
TENSILE STRENGTH |
MO | ASTM D-882 |
Mpa | 6.0 | 6.0 | |
TD | 12.0 | 12.0 | ||||
ELONGATION AT BREAK |
MO | % | 120 | 160 | ||
TD | 40 | 40 | ||||
HEAT SHRINKAGE (120℃/15min) |
MO | ASTM D-1204 |
% | 4.0 | 4.0 | |
TD | 1.5 | 1.5 | ||||
WET TENSION |
IN | ASTM D-2578 |
mN/m | 39 | 39 | |
OUT | ||||||
HAZE | ASTM D-1003 |
% | 83.0 | 90.0 | ||
HEAT SEALING TEMP | 2kg/1second | ℃ | 120 | |||
C.O.F | IN/IN | ASTM D-1894 |
0.61 | 0.60 | ||
OUT/OUT | 0.62 | 0.60 |