BOPP >> 유백필름용

GRADE WO WG
Properties ITEM METHOD UNIT RESULT(대표값임) RESULT(대표값임)
THICKNESS(두께) 포인트법 30 30
TENSILE
STRENGTH
(파단인장강도)
MO ASTM
D-882
Mpa 6.0 6.0
TD 12.0 12.0
ELONGATION
AT BREAK
(파단신장률)
MO % 120 160
TD 40 40
HEAT
SHRINKAGE
(120℃/15min)
(가열치수변화율)
MO ASTM
D-1204
% 4.0 4.0
TD 1.5 1.5
WET
TENSION
(습윤장력)
IN ASTM
D-2578
mN/m 39 39
OUT    
HAZE
(흐림도)
ASTM
D-1003
% 83.0 90.0
HEAT SEALING TEMP 2kg/1초 120  
C.O.F
(마찰계수)
IN/IN ASTM
D-1894
  0.61 0.60
OUT/OUT   0.62 0.60